Effects of Surface Treatments on Piston Ring Friction Force and Wear Riken Corporation
- Format:
- Conference/Event
- Author/Creator:
- Yoshida, Hideki, author.
- Conference Name:
- International Congress & Exposition (1990-02-26 : Detroit, Michigan, United States)
- Language:
- English
- Physical Description:
- 1 online resource
- Place of Publication:
- Warrendale, PA SAE International 1990
- Summary:
- Friction and scuff resistance of ceramic coatings (K-ramic and ion plating) for rings was studied by using a basic wear test machine. Ceramic coatings have been recently remarked for their high heat and wear resistances.Friction force under firing condition was also measured by Furuhama's movable liner method to evaluate piston ring coatings. Ceramic coatings showed lower friction force than the conventional coatings of chromium plate and molybdenum spray coat. A durability test was also conducted to evaluate the wear resistance. Ion plating has the lowest friction with excellent wear resistance, and accordingly is a promising surface treatment for piston rings
- Notes:
- Vendor supplied data
- Publisher Number:
- 900589
- Access Restriction:
- Restricted for use by site license
The Penn Libraries is committed to describing library materials using current, accurate, and responsible language. If you discover outdated or inaccurate language, please fill out this feedback form to report it and suggest alternative language.