Chapter 23-Erosion, Cavitation, and Fretting / JR. Schully, WA. Glaeser.

Format:
Book
Author/Creator:
Schully, JR., author.
Glaeser, WA., author.
Contributor:
American Society for Testing and Materials.
ASTM International.
Series:
Journal of ASTM International. Manual Series ; MNL11029M.
ASTM manual series ; MNL11029M
Language:
English
Subjects (All):
Ultrasonic waves--Industrial applications.
Ultrasonic waves.
Cavitation.
Ultrasonic equipment--Design and construction.
Ultrasonic equipment.
Physical Description:
1 online resource (5 pages) : illustrations, figures, tables.
Volume 2005, Issue 20 (January 2005)
Other Title:
ASTM digital library.
Place of Publication:
West Conshohocken, Pa. : ASTM International, 2005.
System Details:
Mode of access: World Wide Web.
text file PDF
Summary:
SOLID PARTICLE and liquid drop erosion are surface removal processes caused by impingement of solid particles or droplets carried in a moving gas or liquid stream against a surface. Erosion can also occur when the surface is the moving body impacting suspended particles or drops, as happens on a helicopter blade moving through rain.
Notes:
"ASTM Stock Number: MNL11029M".
Includes bibliographical references 15.
Electronic reproduction. W. Conshohocken, Pa. : ASTM International, 2005. Mode of access: World Wide Web. System requirements: Web browser. Access may be restricted to users at subscribing institutions.
Description based on publisher's website, viewed May 03, 2017.
ISBN:
9780803145559 (e-ISBN)
9780803120983
0803120982
Access Restriction:
Restricted for use by site license.

The Penn Libraries is committed to describing library materials using current, accurate, and responsible language. If you discover outdated or inaccurate language, please fill out this feedback form to report it and suggest alternative language.

My Account

Shelf Request an item Bookmarks Fines and fees Settings

Guides

Using the Library Catalog Using Articles+ Library Account